ASTM B537-22 img
Aktiv Normen | Herausgegeben: 01.10.2022

ASTM B537-22

Standard Practice for Rating of Electroplated Panels Subjected to Atmospheric Exposure

Verfügbare Sprachen: Englisch

Verfügbare Ausführung: Sicheres Online-PDF, Norm und Redline – Sicheres Online-PDF, Gedruckt, Gedruckt + redline

ab 62.20 EUR im E-Shop anzeigen

Detailinformationen

Bezeichnung: ASTM B537-22

Ausgabedatum: 01.10.2022

Seiten: 8

Land: Amerikanische technische Norm

Wo ist es zu kaufen?

Erhältlich auf www.technormen.de

Annotation

This practice covers the recommended method for rating the condition of electroplated test panels subjected to corrosive environments for test purposes. This method is used with standard-sized panels exposed on standard ASTM racks at outdoor test sites in both natural atmospheres and accelerated test conditions. This practice refers only to decorative-protective coatings that are cathodic to the substrate such as nickel/chromium or copper/nickel/chromium on steel or zinc die castings, and is not intended for use with anodic sacrificial coatings such as zinc and cadmium on steel. Any modifications needed to adapt the method to rating actual production parts are not considered here. Panels shall be assigned separate rating numbers based on the ability of the coating to protect the substrate from corrosion (protection rating), and the overall appearance of panels as affected by deterioration of the coating itself (appearance rating). Accordingly, rating numbers shall be derived from the type of defect that exists, that is: (1) protection defects, which include crater rusting, pinhole rusting, rust stains, blisters, and other defects that involve basis metal corrosion; and (2) appearance defects, which include surface pits, ""crow´s feet,"" crack patterns, surface stains, tarnishes, and other defects that detract from commercial acceptability as to appearance. Inspection should be made in the as-is condition, and defects to be taken into account are only those that can be seen with the unaided eye at normal reading distance.


Keywords:
atmospheric exposure, corrosion rating, electroplated deposits,, ICS Number Code 25.220.40 (Metallic coatings)
Loading
Cookies Cookies

Potřebujeme Váš souhlas k využití jednotlivých dat, aby se Vám mimo jiné mohli ukazovat informace týkající se Vašich zájmů. Souhlas udělíte kliknutím na tlačítko „OK“.

Souhlas můžete odmítnout zde.

Zde máte možnost přizpůsobit si nastavení souborů cookies v souladu s vlastními preferencemi.

Potřebujeme Váš souhlas k využití jednotlivých dat, aby se Vám mimo jiné mohli ukazovat informace týkající se Vašich zájmů.