ASTM B408-22 img
Active standard | Published: 01/05/2022

ASTM B408-22

Standard Specification for Nickel-Iron-Chromium Alloy Rod and Bar

Available languages: English

Available design: Online Secure PDF, Standard + Redline - Online secure PDF, Print design, Print + redline

from 62.20 EUR show on eshop

Detail information

Designation: ASTM B408-22

Publication date: 01/05/2022

Pages: 6

Country: American technical standard

Where to buy?

You can buy at www.mystandards.biz

Anotation

This specification covers nickel-iron-chromium alloys UNS N08120, UNS N08800, UNS N08810, UNS N08811, and UNS N08890 in the form of hot-worked and cold-worked rod and bar. The material shall be subjected to heat treatment, and its composition shall conform to the chemical requirements for nickel, chromium, iron, manganese, carbon, copper, silicon, sulfur, aluminum, titanium, columbium, molybdenum, niobium, tantalum, phosphorus, tungsten, cobalt, nitrogen, and boron. The material shall conform to mechanical property requirements for tensile strength, yield strength, and elongation. Test methods (chemical analysis, tension test, grain size test) shall be performed in accordance to referenced ASTM documents itemized herein.


Keywords:
bar, rod, UNS N08120, UNS N08800, UNS N08801, UNS N08810, UNS N08811, UNS N08890,, ICS Number Code 77.150.40 (Nickel and chromium products)
Loading
Cookies Cookies

Potřebujeme Váš souhlas k využití jednotlivých dat, aby se Vám mimo jiné mohli ukazovat informace týkající se Vašich zájmů. Souhlas udělíte kliknutím na tlačítko „OK“.

Souhlas můžete odmítnout zde.

Zde máte možnost přizpůsobit si nastavení souborů cookies v souladu s vlastními preferencemi.

Potřebujeme Váš souhlas k využití jednotlivých dat, aby se Vám mimo jiné mohli ukazovat informace týkající se Vašich zájmů.