ASME STP-PT-086:2017 img
Aktivní norma | Vydána: 23.04.2026

ASME STP-PT-086:2017

Effect of High Temperatures and Fit-Up of Riveted Joints on Steel Rivets

Dostupné jazyky: Anglicky

Dostupné provedení: Zabezpečené PDF, Tištěné

od 1 499.30 CZK zobrazit na eshopu

Podrobné informace

Označení: ASME STP-PT-086:2017

Datum vydání: 23.04.2026

Stran: 28

Země: Americká technická norma

Kde koupit?

Můžete zakoupit na eshop.normservis.cz

Anotace

The objective of this study was to evaluate the effects on rivet properties based on maximum hot rivet driving temperatures, plate fit-up, rivet-hole clearances and joint tightness. The most urgent need was to establish whether heating rivets to 2250 degrees F (1230 degrees C) for driving had a detrimental effect on final rivet mechanical properties compared with rivets heated at 1950 degrees F (1065 degrees C). At present, the 2017 Edition of the BPVC, Section I (1) has limited the maximum temperature for hot riveting to 2250 degrees F (1230 degrees C). However, this maximum driving temperature has been challenged by others in the past who have maintained the maximum temperature should be 1950 degrees F (1065 degrees C). See more
Loading
Cookies Cookies

Potřebujeme Váš souhlas k využití jednotlivých dat, aby se Vám mimo jiné mohli ukazovat informace týkající se Vašich zájmů. Souhlas udělíte kliknutím na tlačítko „OK“.

Souhlas můžete odmítnout zde.

Zde máte možnost přizpůsobit si nastavení souborů cookies v souladu s vlastními preferencemi.

Potřebujeme Váš souhlas k využití jednotlivých dat, aby se Vám mimo jiné mohli ukazovat informace týkající se Vašich zájmů.